What Is Battery cell?

Nov 25, 2025

Leave a message

What Is Battery cell?

 

Cell Structure

 

A single battery, also known as a "cell", is the smallest unit of a battery system. It is mainly composed of cathode (Cathode Electrode), anode (Anode Electrode), electrolyte (Electrolyte), separator (Separator), and case (Case), as shown in Figure 7-1.

 

Figure 7-1 Battery Cell Structure

The electrode sheet of a lithium-ion cell can be categorized as a composite material, mainly consisting of four parts:

 

1)Active material particles that intercalate or deintercalate lithium ions; cathode particles provide the lithium source, while anode particles accept lithium ions.

 

2)The conductive phase (carbon gel phase) formed by the mixture of conductive agent and current collector, with the binder serving a bonding function; the coating conducts electrons through the current collector and conductive agent.

 

3)Pores filled with electrolyte, which serve as channels for lithium-ion transport within the electrode sheet.
 

4)Current collector.

 

During the electrochemical process, the electrode coating mainly involves the following 4 processes:

 

1)Electron transport.

 

2)Ion transport.

 

3)Charge exchange at the electrolyte/electrode particle interface, i.e., the electrochemical reaction.

 

4)Diffusion of lithium ions within the solid phase. In the microstructure of the electrode sheet, particle size and distribution affect the lithium-ion diffusion path and the specific surface area of the electrochemical reaction; pore size and distribution affect the transport process of the electrolyte; porosity affects the amount of active material and the specific surface area of the electrochemical reaction. All these microstructural characteristics ultimately influence battery performance.

 

Cathode Structure

 

The cell cathode is mainly composed of cathode materials such as LiCoO₂, conductive agent, binder (PVDF), and current collector (aluminum foil), as shown in Figure 7-2.

Figure 7-2 Battery Cell Cathode Structure

For lithium-ion batteries, the cathode current collector is usually aluminum foil and the anode current collector is copper foil. To ensure the stability of the current collector inside the battery, the purity of both must be above 98%. The reasons why lithium-ion batteries use aluminum foil for the cathode and copper foil for the anode are the following 3 points:

 

1)Copper and aluminum have good electrical conductivity, soft texture, and low price. The working principle of a lithium-ion battery is an electrochemical device that converts chemical energy into electrical energy. In this process, a medium is required to transfer the chemical energy into electrical energy, which requires a conductive material. Among common materials, metals have the best electrical conductivity, and among metals, copper and aluminum offer both excellent conductivity and relatively low price in the form of copper foil and aluminum foil. In lithium-ion batteries, there are mainly two processing methods: winding and stacking. Compared with stacking, winding requires the electrode sheets used to prepare the battery to have a certain flexibility to ensure that the electrode sheets do not become brittle or break during winding. Among metal materials, copper and aluminum foils are soft, relatively hard copper/aluminum foils are expensive, copper and aluminum foils are relatively cheap, and copper and aluminum resources are abundant worldwide.

 

2)Copper and aluminum foils are also relatively stable in air. Aluminum easily reacts chemically with oxygen in the air to form a dense oxide film on the surface, preventing further reaction of the aluminum. This oxide film of copper/aluminum also provides a certain protective effect on aluminum in the electrolyte. Copper itself is relatively stable in air and basically does not undergo chemical reactions in dry air.

 

3)The cathode and anode potentials of lithium-ion batteries determine that aluminum foil is used for the cathode and copper foil for the anode, and they cannot be reversed. The cathode potential is high, and copper foil is easily oxidized at high potential, while aluminum has a high oxidation potential and a dense oxide film on its surface layer, which also provides good protection for the internal aluminum.

 

In the crystal lattice of metallic aluminum, copper and aluminum have sizes similar to Li and can easily form intermetallic compounds with Li such as LiAl. Li and Al can not only form the alloy with the chemical formula LiAl, but may also form Li₉Al₄,Li₃Al₂,Li₅Al and Li₂Al alloy layers. These alloy layers consume a large amount of Li and damage the structure and morphology of Al itself, so it cannot be used as the anode current collector of lithium-ion batteries; while Cu undergoes very little dissolution during battery charge-discharge and maintains structural and electrochemical stability, making it suitable as the anode current collector for lithium-ion batteries. For copper foil at 3.5V, the polarization current begins to increase significantly and rises linearly, with intensified oxidation, indicating that Cu also begins to dissolve in the battery; while for aluminum foil across the entire polarization potential range, the polarization current is small and stable, with no obvious corrosion phenomena observed, maintaining electrochemical stability. Since the dissolution amount of Al in the cathode potential range of lithium-ion batteries is extremely small and electrochemical stability can be maintained, it is suitable as the cathode current collector for lithium-ion batteries.

 

The oxide layer on copper/aluminum surfaces belongs to semiconductors and conducts electrons; if the oxide layer is too thick, the impedance is large; while the aluminum oxide layer on the aluminum surface is an insulator and cannot conduct electricity, but because it is very thin, electron conduction is achieved through the tunneling effect; if the oxide layer is thick, the conductivity of copper/aluminum foil is poor or even insulating. Generally, copper/aluminum foil needs to be cleaned of the oxide layer before use to remove oil on the one hand and thick oxide layers on the other. The cathode potential is high, and the aluminum oxide layer is very dense, which can prevent oxidation of the current collector. Oxide layers of copper/nickel etc. are relatively loose, easily preventing the current collector and providing better battery performance. At the same time, the anode potential of lithium-ion batteries is low, and copper/nickel will undergo oxidation reactions, with oxidation/copper/de-lithiation reactions occurring on the copper/nickel surface, while aluminum undergoes LiAl alloying at high potential.

 

The current collector requires pure composition. Impurities in Al will make the surface film less dense and cause pitting corrosion, and even more severely, destruction of the surface film leads to the formation of LiAl alloy.

 

The current collector requires pure composition. Impurities in Al will cause the surface film to be less dense, leading to pitting corrosion, and even worse, destruction of the surface film results in the formation of LiAl alloy.

 

Battery cell

 

For lithium-ion batteries, the cathode aluminum foil has been reduced from 16μm to 14μm, then to 12μm, and now 10μm aluminum foil is already in mass production, with some even using 8μm; for the anode copper foil, due to its inherently better flexibility, its thickness has been reduced from the previous 12μm to 10μm, then to 8μm, and currently a large portion of batteries are mass-produced using 6μm, while some manufacturers are developing 5μm/4μm which are also potentially usable. Since lithium-ion batteries have high purity requirements for the copper foil used, the material density is basically at the same level. As the thickness under development decreases, the areal density decreases accordingly, and the weight of the battery naturally becomes lighter and lighter, which meets the demand for lithium-ion batteries.

 

For current collectors, in addition to their thickness and weight affecting lithium-ion batteries, the surface properties of the current collector also have a significant impact on battery production and performance. Especially for the anode current collector, due to defects in preparation technology, the copper foils on the market are mainly single-sided roughened, double-sided roughened, and double-sided coarsened varieties. This asymmetric two-sided structure will lead to asymmetric contact resistance of the anode coating on both sides, thereby preventing uniform release of anode capacity on both sides; at the same time, the asymmetry on both sides will also cause inconsistent adhesion strength of the anode coating, resulting in severely unbalanced charge-discharge cycle life of the anode coating on both sides, which in turn accelerates the capacity decay of the battery.

 

The cathode formulation of a single cell is the key core technology of the cell. Below is an example:

 

1)LiCoO₂ (10μm): 96.0%.

2)Conductive agent (Carbon ECP): 2.0%.

3)Binder (PVDF 761): 2.0%.

4)Adhesion promoter (NMP): The weight ratio of solid substances is approximately 810:1496.

 

Cathode formulation precautions:

 

1)Cathode slurry viscosity control at 6000cP (1cP = 1mPa · s) (temperature 25℃).

2)The weight of NMP must be appropriately adjusted to meet the viscosity requirement.

3)Pay special attention to the influence of temperature and humidity on viscosity.

 

Cathode material lithium cobalt oxide: Cathode active material, lithium ion source, provides lithium source for the battery. Non-polar substance, irregular shape, particle size D50 generally 6~8μm, moisture content ≤0.2%, usually alkaline, pH 10~11.

 

Cathode material lithium manganese oxide: Non-polar substance, irregular shape, particle size D50 generally 5~7μm, moisture content ≤0.2%, usually weakly alkaline, pH around 8.

 

Conductive agent: Chain-like substance, moisture content <1%, particle size generally 1~5um.Superconductive carbon black with excellent conductivity is usually used, such as KetjenblackCarbon ECP and ECP600JD. lts function is to improve the conductivity of the cathode material,compensate for the electronic conductivity of the cathode active material; increase the electrolyteabsorption of the cathode sheet, expand the reaction interface, and reduce polarization.

 

Binder (PVDF): Non-polar substance, chain-like, molecular weight ranging from 300000 to3000000; molecular weight decreases after water absorption, resulting in poorer adhesion. lt isused to bond lithium cobalt oxide, conductive agent, and aluminum foil or aluminum mesh togethelAdhesion promoter (NMP): Weakly polar liquid, used to dissolve/swell PVDF and simultaneouslydilute the slurry.


Current collector (cathode tab): Made of aluminum foil or aluminum strip.

 

Anode Structure

Figure 7-3 Negative Electrode Structure of Battery Cell

The cell anode structure consists of graphite material, conductive agent, thickener (CMC), binder (SBR), and current collector (copper foil), as shown in Figure 7-3.

The anode formulation of a single cell is also one of the key core technologies of the cell, typically as follows:

 

1)Anode material (graphite): 94.5%.

2)Conductive agent (Carbon ECP): 1.0% (Ketjenblack).

3)Binder (styrene-butadiene rubber latex, SBR): 2.25%.

4)Thickener (carboxymethyl cellulose, CMC): 2.25%.

5)Water: The weight ratio of solid substances is 1600:1417.5.

 

Anode formulation precautions:

 

1)Anode slurry viscosity control at 5000~6000cP (temperature 25℃).

2)The weight of water needs to be appropriately adjusted to meet the viscosity requirement.

3)Pay special attention to the influence of temperature and humidity on viscosity.

 

Graphite: Anode active material, the main substance constituting the anode reaction, mainly divided into two major categories: natural graphite and artificial graphite. Non-polar substance, easily contaminated by non-polar substances, easily dispersed in non-polar substances; not easy to absorb water, nor easy to disperse in water. Contaminated graphite, after being dispersed in water, tends to re-agglomerate. The general particle size D50 is around 20μm. Particle shapes are diverse and mostly irregular, mainly spherical, flaky, fibrous, etc.

 

Functions of conductive agent:

 

1)Improve the conductivity of the anode sheet and compensate for the electronic conductivity of the anode active material.

2)Increase reaction depth and utilization rate.

3)Prevent the generation of dendrites.

4)Utilize the liquid-absorbing capacity of conductive materials to increase the reaction interface and reduce polarization (can be added or not according to graphite particle size distribution).

 

cathode and anode

 

Additives: Reduce irreversible reactions, increase bonding strength and slurry viscosity, and prevent slurry sedimentation.

Thickener/anti-settling agent (CMC): High molecular compound, easily soluble in water and polar solvents.

Isopropanol: Weakly polar substance; after addition, it can reduce the polarity of the binder solution, improve the compatibility between graphite and binder solution; has strong defoaming effect; easily catalyzes the cross-linking of binder network and improves bonding strength.

Ethanol: Weakly polar substance; after addition, it can reduce the polarity of the binder solution, improve the compatibility between graphite and binder solution; has strong defoaming effect; easily catalyzes linear cross-linking of binder and improves bonding strength (the functions of isopropanol and ethanol are essentially the same; when mass-producing, cost factors can be considered to choose which one to add).

Water-based binder (SBR): Bonds graphite, conductive agent, additives, and copper foil or copper mesh together; linear chain emulsion molecule, extremely soluble in water and polar solvents.

Deionized water (or distilled water): Diluent, added in appropriate amount, can change the fluidity of the slurry.

Anode tab: Made of copper foil or copper strip.